PHYSICS RESOURCES DATABASE
ELECTRICAL, MAGNETIC & OPTICAL PROPERTIES
RESISTIVITIES
R = r L / A
Values at ~20 °C
|
Substance |
Resistivity r (W .m) |
|
Aluminum |
2.8x10-8 |
|
Brass |
~8x10-8 |
|
Constantan (60% Cu, 40% Ni) |
~44x10-8 |
|
Copper |
1.7x10-8 |
|
Iron |
~10x10-8 |
|
Manganin (~84% Cu, ~12% Mn, ~4% Ni) |
44x10-8 |
|
Mercury |
96x108 |
|
Nichrome (~59% Ni, ~ 23% Cu, ~ 16% Cr) |
100x10-8 |
|
Platinum |
10x10-8 |
|
Silver |
1.6X10-8 |
|
Tungsten |
5.5x10-8 |
|
Carbon |
3.5x10-5 |
|
Germanium |
0.46 |
|
Silicon |
100-1000 |
|
Glass |
1010-1014 |
|
Neoprene |
109 |
|
Polyethylene |
~108 |
|
Polystyrene |
~109 |
|
Porcelain |
~ 1011 |
|
Teflon |
1014 |
|
Blood |
1.5 |
|
Fat |
25 |
Return to Electrical, ...Properties